Hongkyu Kim - Old Bridge NJ, US Ronald Walter Mason - Painted Post NY, US Himanshu Chandrakant Shah - Painted Post NY, US David Alan Tammaro - Painted Post NY, US
Assignee:
Corning Incorporated - Corning NY
International Classification:
B65D 85/48 B32B 37/02 B32B 17/06
US Classification:
206454, 156 60, 156344, 428426
Abstract:
Described herein are methods for protecting glass with the use of glassine paper.
George L. Collins - Maplewood NJ Kurt F. Wissbrun - Short Hills NJ Hongkyu Kim - Madison NJ
Assignee:
Hoechst Celanese Corporation - Somerville NJ
International Classification:
C08G 210
US Classification:
528230
Abstract:
There are provided new elastomeric copolymers of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0. 005 to 0. 15 wt. %, preferably about 0. 05 to 0. 12 wt. % of 1,4-butanediol diglycidyl ether or butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. The elastomeric copolymers may be prepared by mixing said monomers in a substantially dry state and under an inert atmosphere with a cationic polymerization catalyst, e. g, p-nitrobenzenediazonium tetrafluoroborate. The elastomeric copolymers have a strong interaction with moldable, crystalline acetal polymers comprising at least 85 mol % of polymerized oxymethylene units and may be used as a blending agent with such crystalline acetal polymers or as a bonding agent to improve the adhesiveness of the crystalline acetal polymer to other materials.
George L. Collins - Maplewood NJ Kurt F. Wissbrun - Short Hills NJ Hongkyu Kim - Madison NJ
Assignee:
Hoechst Celanese Corp. - Somerville NJ
International Classification:
C08G 224
US Classification:
528230
Abstract:
There are provided new elastomeric copolymers of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0. 005 to 0. 15 wt. %, preferably about 0. 05 to 0. 12 wt. % of 1,4-butanediol diglycidyl ether or butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. The elastomeric copolymers may be prepared by mixing said monomers in a substantially dry state and under an inert atmosphere with a cationic polymerization catalyst, e. g. , p-nitrobenzenediazonium tetrafluoroborate. The elastomeric copolymers have a strong interaction with moldable, crystalline acetal polymers comprising at least 85 mol % of polymerized oxymethylene units and may be used as a blending agent with such crystalline acetal polymers or as a bonding agent to improve the adhesiveness of the crystalline acetal polymer to other materials.
Kurt F. Wissbrun - Short Hills NJ Hongkyu Kim - Basking Ridge NJ George L. Collins - Maplewood NJ Diane Terrone - Toms River NJ
Assignee:
Hoechst Celanese Corp. - Somerville NJ
International Classification:
C08L 6102 C08F28306 C08G 6532
US Classification:
525398
Abstract:
There are provided new moldable blends of a normally crystalline acetal polymer and a normally non-crystalline elastomeric copolymer of about 15 to 45 mol %, preferably about 25 to 35 mol % of trioxane, about 55 to 85 %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0. 005 to 0. 15 wt. %, preferably about 0. 05 to 0. 12 wt. % of 1,4-butanediol diglycidyl ether or butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer.
George L. Collins - Maplewood NJ Hongkyu Kim - Basking Ridge NJ William M. Pleban - Stanhope NJ
Assignee:
Hoechst Celanese Corp. - Somerville NJ
International Classification:
B32B 2738 C08G 210
US Classification:
428414
Abstract:
There are provided new articles comprising elements having surfaces bonded together with a bonding resin which is an elastomeric copolymer of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0. 005 to 0. 15 wt. %, preferably about 0. 05 to 0. 12 wt. % of 1,4-butanediol diglycidyl ether or butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. Preferably, at least one of said surfaces, and more preferably at least two of said surfaces bonded to each other are of a crystalline acetal polymer comprising at least 85 mol % of polymerized oxymethylene units.